Nsuku zonke ngifunde kancane nge-PCB futhi ngikholwa ukuthi ngingaba ngochwepheshe kakhulu emsebenzini wami. Namuhla, ngifuna ukwethula izinhlobo eziyi-16 zezinkinga zokushisela ze-PCB ezivela ezicini zokubukeka, izingozi, izimbangela.
1.Pseudo Soldering
Izici zokubukeka:kukhona umngcele omnyama osobala phakathi kwe-solder nengxenye yomthofu noma i-copper foil, futhi i-solder ifinyelele emngceleni
Izingozi:ayikwazi ukusebenza kahle
Izimbangela:1) izintambo eziholayo zezingxenye azihlanzwa kahle, azifakwanga kahle noma zifakwe i-oxidized.
2) I-PCB ayihlanzekile, futhi izinga lokufafazwa kwe-flux alilungile
2. Ukuqoqwa kwe-solder
Izici zokubukeka:Amalunga e-solder akhululekile, amhlophe futhi abuthuntu.
Izingozi:amandla mechanical akwanele, may virtual Welding
Izimbangela:1) izinga eliphansi le-solder.2) izinga lokushisa elinganele le-welding.3) lapho i-solder ingaqinisiwe, ukuhola kwengxenye kuyaxega.
3.I-solder eningi kakhulu
Izici zokubukeka:Ubuso be-solder buyi-convex
Izingozi:I-waste solder futhi ingase ibe nokukhubazeka
Izimbangela:ukuhoxiswa kwe-solder kuphuze kakhulu
4. I-solder encane kakhulu
Izici zokubukeka:Indawo yokushisela ingaphansi kuka-80% we-welding pad, futhi i-solder ayenzi indawo eguquguqukayo ebushelelezi.
Izingozi:amandla emishini awanele,
Izimbangela:I-1) ukungahambi kahle kwe-solder noma ukuhoxiswa kwe-solder ngaphambi kwesikhathi. 2) i-flux enganele.3) isikhathi sokushisela sifushane kakhulu.
5. Ukushisela i-rosin
Izici zokubukeka:Kukhona izinsalela ze-rosin ku-weld
Izingozi:amandla okulimaza ayanele, ukuqhutshwa kubi, kungenzeka uma kuvuliwe noma kuvaliwe
Izimbangela:1) umshini wokushisela ngokweqile noma ukwehluleka.2) isikhathi esinganele sokushisela nokushisa.3) ifilimu ye-oxide ye-surface ayisusiwe.
6. hyperthermia
Izici zokubukeka:I-solder ehlangene imhlophe, ngaphandle kokucwebezela kwe-metallic, ingaphezulu lilukhuni.
Izingozi:Kulula ukukhipha i-welding pad futhi unciphise amandla
Izimbangela:i-solder iron iron inamandla kakhulu futhi isikhathi sokushisa side kakhulu
7. kubanda ukushisela
Izici zokubukeka:indawo engaphezulu ibe yizinhlayiya ze-tofu slag, ngezinye izikhathi ingase ibe nemifantu
Izingozi:Amandla aphansi kanye nokungahambi kahle kukagesi
Izimbangela:i-solder iyancibilika ngaphambi kokuqina.
8. Ukungena okubi
Izici zokubukeka:isikhombimsebenzisi phakathi kwe-solder ne-welding inkulu kakhulu, ayibushelelezi
Izingozi:Ukuqina okuphansi, okungahambeki noma okuphakathi
Izimbangela:I-1) izingxenye ze-welding azihlanzwa 2) i-flux enganele noma ikhwalithi embi.3) izingxenye ze-welding azishisi ngokugcwele.
9. i-dissymmetry
Izici zokubukeka:ipuleti le-solder aligcwele
Izingozi:Amandla okulimala anganele
Izimbangela:1) uketshezi lwe-solder olumpofu.2) ukugeleza okunganele noma izinga eliphansi.3) ukushisisa okunganele.
10. Ukulahlekelwa
Izici zokubukeka:izintambo zokuhola noma izingxenye zingasuswa
Izingozi:kubi noma ungaqhubeki
Izimbangela:I-1) ukunyakaza okuholayo kubangela ukungabi nalutho ngaphambi kokuqiniswa kwe-solder.2) umthofu awuphathwa kahle (umpofu noma awungenwanga)
11.I-Solder ukuqagela
Izici zokubukeka:kuvele ku-cusp
Izingozi:Ukubukeka okubi, kulula ukubangela amabhuloho
Izimbangela:1) i-flux encane kakhulu kanye nesikhathi sokushisisa eside kakhulu.2) ukuphuma okungafanele I-engeli ye-solder iron
12. Ukuxhumana kwebhuloho
Izici zokubukeka:Uxhumano lwezintambo eziseduze
Izingozi:Isifunda esifushane sikagesi
Izimbangela:1) solder ngokweqile. 2) ukuphuma okungalungile I-Angle yensimbi yokunamathisela
13.Phina Izimbobo
Izici zokubukeka:Izimbobo ziyabonakala kuma-amplifiers abonakalayo noma aphansi
Izingozi:Amandla anganele kanye nokugqwala okulula kwamalunga e-solder
Izimbangela:igebe phakathi kwentambo yokuhola kanye nembobo yephedi yokushisela inkulu kakhulu.
14.Igwebu
Izici zokubukeka:impande yocingo oluholayo ine-spitfire solder uplift kanye nomgodi wangaphakathi
Izingozi:Ukuqhutshwa kwesikhashana, kodwa kulula ukubangela ukuqhutshwa okubi isikhathi eside
Izimbangela:1) igebe elikhulu phakathi komthofu kanye nembobo yephedi yokushisela.2) ukungena komthofu okungekuhle.3) ukuxhuma kwamaphaneli amabili embobeni kuthatha isikhathi eside ukushisela, futhi umoya ongaphakathi embobeni uyakhula.
15. I-copper foil phezulu
Izici zokubukeka:ucwecwe lwethusi kusukela ephrintiwe ebhodini stripping
Izingozi:I-pcb yonakele
Izimbangela:isikhathi sokushisela side kakhulu futhi izinga lokushisa liphezulu kakhulu.
16. Ukucwecwa
Izici zokubukeka:i-solder ephuma ku-foil yethusi (hhayi i-copper foil kanye ne-PCB stripping)
Izingozi:I-circuit breaker
Izimbangela:ukumbozwa kahle kwensimbi ku-welding pad.